Cellulose Acetate
CROW logo
Cellulose Acetate
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Cellulose
COMMON NAMESCellulose Acetate
STRUCTURE BASED NAME
ACRONYMS CA
CAS # 9035-69-2 (Diacetate)
9012-09-3 (Triacetate)
CurlySMILES
 

IDENTIFIERS OF MONOMER(S)

CAS # N/A
COMMON NAMESN/A
SMILES N/A
Std. InChI N/A
Std. InChIKey N/A
STRUCTURE
Cellulose Acetate
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGE*PREFERRED
Molar Volume VmmL mol-1 N/A 
Density ρg mL-1 1.29 - 1.311.30
Solubility Parameter δMPa1/2 22 - 2824
Molar Cohesive Energy EcohJ mol-1 N/A 
Glass Transition Temperature TgK 448 - 473
460 - 490
460 (DP 2.9)
480 (DP 2.5)
Molar Heat Capacity CpJ (mol K)-1   
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone 1.47 - 1.48 1.48
 

Thermo-Physical Properties: Calculated Data

PROPERTY UNIT VALUE / RANGE PREFERRED
Molecular Weight of Repeat unitg mol-1  
Van-der-Waals Volume VvWmL mol-1  
Molar Volume Vm mL mol-1 N/A
Density ρg mL-1   
Solubility Parameter δMPa1/2   
Molar Cohesive Energy EcohJ mol-1 N/A 
Glass Transition Temperature TgK   
Molar Heat Capacity CpJ (mol K)-1   
Entanglement Molecular Weight Meg mol-1   
Index of Refraction nnone   

*The properties depend on the total degree of substitution on the repeating glucose units. The degree of acetylation is typically in the range of 2.4 - 2.9.

back to top